英语翻译With CO2 shielding ,best toughness was obtained in the uphill welding position and with two passes per layer,if all the test temperature rage is considered.ANSI/AWS A5.29-98 E91-T5-K2/K2M and E101T5-K3/K3M impact requirements were very co

来源:学生作业帮助网 编辑:作业帮 时间:2024/05/04 12:29:25

英语翻译With CO2 shielding ,best toughness was obtained in the uphill welding position and with two passes per layer,if all the test temperature rage is considered.ANSI/AWS A5.29-98 E91-T5-K2/K2M and E101T5-K3/K3M impact requirements were very co
英语翻译
With CO2 shielding ,best toughness was obtained in the uphill welding position and with two passes per layer,if all the test temperature rage is considered.
ANSI/AWS A5.29-98 E91-T5-K2/K2M and E101T5-K3/K3M impact requirements were very comfortably satisfied in all the welding conditions,and the all-weld-metal chemical composition met the E101T5-K3/K3M requirement.

英语翻译With CO2 shielding ,best toughness was obtained in the uphill welding position and with two passes per layer,if all the test temperature rage is considered.ANSI/AWS A5.29-98 E91-T5-K2/K2M and E101T5-K3/K3M impact requirements were very co
一楼的机器翻译痕迹也过于明显了吧,从第二段来看应该是对工厂焊接工艺流程及规范的检验报告,第一段指的可能是气体保护焊
在二氧化碳保护下,如果所有的检验温度范围都被考虑到的话(这里应该是range,而不是rage),最佳强度是由上坡口焊接位置和每层两道焊得到的
美国国家标准协会(American National Standards Institute)/美国焊接协会(America welding Society) A5.29-98 E91-T5-K2/K2M 和E101T5-K3/K3M冲击性能要求在所有的焊接环境下都能很好的得到满足,并且所有的焊剂都达到E101T5-K3/K3M要求

藉由 CO2 屏隔,最好的有黏性在上坡的焊接位置被获得而且由于每层二个途径,如果所有的测试温度愤怒被考虑。
ANSI/AW a5.29-98 E91-T5-K2/K2 M 和 E101 T5-K3/K3 M 冲击需求非常安乐地被满意在所有的那焊接情况 , 和所有者-焊接处-遇见 E101 的金属制的化学作文 T5-K3/K3 M 需求。...